Concrete Floor and Wall Systems

Protection from the Bottom to the Top

From JPCL, December 2021

By Kevin Kipp, Hardig Industrial Services

Owners of one U.S. food and beverage manufacturing facility decided to refurbish a large oven room in one of their facilities. To protect the refinished oven room’s concrete walls and floors, the owners decided to install new high-performance coating systems instead of new tiling. This article recaps the oven room refurbishment project from original demolition to completion....


(Login to read the full article)
   

Comment Join the Conversation:

Sign in to our community to add your comments.

Advertisements
 
Tarps manufacturing, Inc.

 
Modern Safety Techniques

 
NLB Corporation

 
Paint BidTracker

 
HoldTight Solutions Inc.

 
Sauereisen, Inc.

 
Strand’s Industrial Coatings

 
CRW

 
 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us