Coating Work at the Cowans Ford Hydroelectric Station

From JPCL, July 2021

By Todd Ceol, Superior Industrial Maintenance Co., LLC

A multi-year coating rehabilitation project was recently completed at a hydroelectric power plant, which caused the selected coating contractor to get creative with its means and methods of completing the required work. This article details how the contractors utilized cranes, barges, an onsite layaway building and a climate-controlled paint shop to finish the job....


(Login to read the full article)
   

Comment Join the Conversation:

Sign in to our community to add your comments.

Advertisements
 
KTA-Tator, Inc. - Corporate Office

 
Sauereisen, Inc.

 
Axxiom Manufacturing

 
HoldTight Solutions Inc.

 
CRW

 
Tarps manufacturing, Inc.

 
Seal for Life/STOPAQ

 
Abrasives Inc.

 
 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us