By Ahsan Chowdhury, Halifax Harbour Bridges; and Kenneth A. Trimber, KTA-Tator, Inc.
There are many unique challenges related to bridge corrosion-protection projects. This article describes the design, implementation, and lessons learned from a pilot program conducted by Halifax Harbour Bridges on the Angus L. Macdonald Bridge in an effort to develop a coating maintenance program that would offer a minimum
25–30-year service life....