Measuring TSA Coating Thickness: Methods and Considerations

From JPCL, April 2019

By Jay Kunick, Fischer Technology, Inc.

Thermally sprayed aluminium (TSA) coatings can offer long-term corrosion protection for atmospheric, offshore structures or marine environments, but accuracy of TSA thickness measurements becomes a critical part of the process in order to maximize the coating’s effectiveness and longevity. This article outlines the measuring methods available and the effects the type of substrate material and other factors have on thickness measurement quality....


(Login to read the full article)
   

Tagged categories: Calibration; Coating inspection; Coating/Film Thickness; Eddy-current thickness gauge; Offshore; Quality Control; Thermal-spray aluminum (TSA)

Comment Join the Conversation:

Sign in to our community to add your comments.

Advertisements
 
Western Technology Inc.

 
Abrasives Inc.

 
PaintSquare

 
CRW

 
Sauereisen, Inc.

 
Tarps manufacturing, Inc.

 
Axxiom Manufacturing

 
KTA-Tator, Inc. - Corporate Office

 
 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us