Three-Coat & Epoxy Mastic Bridge Coating Systems in Adverse Environments

From JPCL, May 2018

By Saiada Fuadi Fancy, Md. Ahsan Sabbir and Kingsley Lau, Florida International University and Dale DeFord, Florida Department of Transportation

This article presents experimental results of coating degradation and corrosion development on three-coat systems and aluminum epoxy mastic repair coatings on steel with various types of surface preparation and subjected to cyclic salt wet-dry exposure cycles....


(Login to read the full article)
   

Tagged categories: Adhesion; Bridges; Coating Materials; Epoxy; Exposure conditions; Multicoat Systems; Performance testing

Comment Join the Conversation:

Sign in to our community to add your comments.

Advertisements
 
GMA Garnet USA

 
Axxiom Manufacturing

 
Abrasives Inc.

 
Tarps manufacturing, Inc.

 
HoldTight Solutions Inc.

 
CRW

 
Western Technology Inc.

 
Sauereisen, Inc.

 
KTA-Tator, Inc. - Corporate Office

 
 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us