Fundamentals of Fusion-Bonded Epoxy Application

From JPCL, April 2018

By David A. Hunter and Sean M. Browning, Pond & Company

FBE coatings can be applied in a manufacturing process which provides a consistent, durable coating for buried application. As with any manufacturing process, diligence in identifying flaws, monitoring temperature and consistency of surface preparation and application are critical to the long-term performance of the materials....


(Login to read the full article)
   

Tagged categories: Coating Application; David Hunter; Fusion bonded epoxy; Paint application; Pipelines

Comment Join the Conversation:

Sign in to our community to add your comments.

Advertisements
 
Abrasives Inc.

 
PaintSquare

 
Western Technology Inc.

 
Axxiom Manufacturing

 
HoldTight Solutions Inc.

 
CRW

 
Sauereisen, Inc.

 
Tarps manufacturing, Inc.

 
 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us