By Hank Bernacki, Zhenwen Fu, Bingquan Li, Denise Lindenmuth and Leo Procopio, The Dow Chemical Company

The challenge with epoxy chemistry is maintaining all of the excellent coating properties such as adhesion, corrosion resistance and chemical/solvent resistance while improving upon its weaknesses such as flexibility, potlife and UV durability. The Type III acrylic/epoxy systems improve upon UV durability, but with slow cure speed and property development. This article describes a new acrylic-epoxy hybrid polymer technology for 2K waterborne coatings that addresses these issues....


(Login to read the full article)
   

Tagged categories: Bisphenol A; Bisphenol A (BPA); Coating Materials; Coating performance; Epoxy; Epoxy amine; UV resistance

Comment Join the Conversation:

Sign in to our community to add your comments.

Advertisements
 
Abrasives Inc.

 
HoldTight Solutions Inc.

 
Axxiom Manufacturing

 
Sauereisen, Inc.

 
KTA-Tator, Inc. - Corporate Office

 
PaintSquare

 
Western Technology Inc.

 
CRW

 
 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us