By Steven Reinstadtler and Robert Wade, Covestro LLC
The evolution of water-based UV-cured wood coating technology has led to the availability of site-applied UV wood floor coatings that replicate the abrasion and stain resistance of their OEM-applied counterparts. This feature covers performance properties and application techniques....