Investigating Failure
Failure of a Bridge Deck Topcoat

From JPCL, November 2016

By Warren Brand, Chicago Corrosion Group, LLC.

...


(Login to read the full article)
   

Tagged categories: Bridges; Coating failure; concrete; Failure analysis; Quality Control; Topcoats; Warren Brand

Comment from LUIS ALFREDO CHACON GUERRERO, (12/19/2016, 9:09 AM)

IS A VALUABLE CONTRIBUTION TO THE STUDY OF THE PATOLOGIES OF COATINGS FAILURES. EXCELLENTE TECHNICAL WORK


Comment from Warren Brand, (12/19/2016, 2:05 PM)

Hi Luis. Thank you very much for your kind words. Happy Holidays.


Comment from David Rasmussen, (12/19/2016, 3:29 PM)

I had a similar situation occur in 2007 involving 700,000 sf of concrete in a converted warehouse. Same conclusion as above. Law Firms involved, binding arbitration, plenty of blame and expenses to go around. Sometimes we learn the hard way. Great article, invaluable info.


Comment from Larry Muzia, (12/20/2016, 9:08 AM)

Excellent report, I am having all our journeymen read the article. Larry Muzia


Comment from Warren Brand, (12/20/2016, 6:12 PM)

Hi David, Hello Larry, Thank you both very much for taking the time to respond and for your kind words.


Comment Join the Conversation:

Sign in to our community to add your comments.

Advertisements
 
Sauereisen, Inc.

 
KTA-Tator, Inc. - Corporate Office

 
Axxiom Manufacturing

 
Western Technology Inc.

 
CRW

 
Tarps manufacturing, Inc.

 
PaintSquare

 
Abrasives Inc.

 
HoldTight Solutions Inc.

 
 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us