Induction Heating for Cold Weather Preheating and Post-Curing Of Liquid Epoxy Coatings On Gas Pipeline Girth Welds

From JPCL, February 2016

By Bruce J. Wiskel, P.E., Pacific Gas & Electric Company; and J. Peter Ault, P.E., Elzly Technology Corporation

The authors discuss the challenges of applying coatings to transmission pipeline when the surface temperature dips below 50 F and determine that the optimum approach for cold weather coating application on girth welds is to use the existing approved epoxy coatings with induction preheat of the pipe during surface preparation, coating application and cure....


(Login to read the full article)
   

Tagged categories: Coating Application; Curing; Epoxy; Girth welds; Heaters; Induction heating; Laboratory testing; Paint application; Performance testing; Pipeline; Pipelines; Site/field testing

Comment Join the Conversation:

Sign in to our community to add your comments.

Advertisements
 
Tarps manufacturing, Inc.

 
Modern Safety Techniques

 
HoldTight Solutions Inc.

 
CRW

 
NLB Corporation

 
Strand’s Industrial Coatings

 
Sauereisen, Inc.

 
Paint BidTracker

 
 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us