by Mike O'Donoghue, Ph. D. and Vijay Datta, M.S., International Paint LLC

The authors compare and contrast the accelerated laboratory autoclave performance of various types of epoxy linings for tank, vessel and pipe spool applications in the oil and gas industry....
(Login to read the full article)

   

Tagged categories: Coating Materials; Formulating; Fracking; Laboratory testing; Mike O'Donoghue; Oil and Gas; Performance testing; Vijay Datta

Comment Join the Conversation:

Sign in to our community to add your comments.

Advertisements
 
Tarps manufacturing, Inc.

 
HoldTight Solutions Inc.

 
Western Technology Inc.

 
Sauereisen, Inc.

 
CRW

 
PaintSquare

 
Axxiom Manufacturing

 
KTA-Tator, Inc. - Corporate Office

 
 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us