Meeting Demands of Gas Exploration: The Evolution of Pipeline Coatings

From JPCL, November 2015

by E. Bud Senkowski, P.E., P.C.S., KTA-Tator, Inc.

This article describes the coating materials, surface preparation requirements and application methods used to protect gas pipelines. It also provides information about the types of polymer-based coatings that are both cost-effective and have a high level of acceptance in the gas pipeline industry....
(Login to read the full article)

   

Tagged categories: Coating Materials; Coating selection; Epoxy; Fracking; Fusion bonded epoxy; Oil and Gas; Paint application; Pipeline; Urethane

Comment from Anthony Asmar, (12/15/2015, 8:30 AM)

Pls, advise what exactly the full system of the polypropylene pipeline coating! Shall epoxy primer applied after surface preparation ? If so, it will not bubble once the pipe heated during application of PE ? Could u provide me with the full system including surface preparation on my e mil: tony_asmar2@hotmail.com. could u pls provide me the product name preferred as well? Best regards.


Comment from John Binder, (1/6/2016, 8:27 AM)

Excellent article. This one is certainly a keeper for my pipe coatings archive.


Comment from Marco Antonio Alvarado Meneses, (1/6/2016, 9:46 PM)

A very good article about pipeline coatigs.


Comment from OM PRAKASH JAT, (1/21/2016, 1:37 AM)

It helps me a lot.


Comment from bill wilson, (2/8/2016, 4:17 PM)

Great resource.I thought you might fine this interesting, Hard is not always tough enough. Specifying pipeline coatings.. this was a resent article in the Technical page of managing aging plants.


Comment Join the Conversation:

Sign in to our community to add your comments.

Advertisements
 
HoldTight Solutions Inc.

 
KTA-Tator, Inc. - Corporate Office

 
CRW

 
PaintSquare

 
Axxiom Manufacturing

 
Abrasives Inc.

 
Tarps manufacturing, Inc.

 
Western Technology Inc.

 
 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us