Influence of UHP Waterjetting on Shop-Primed Steel in New Construction, Part 3

From JPCL, August 2012

by Philippe Le Calvé, DCNS; Jean-Pierre Pautasso, Direction Générale de I’Armement; and Nathalie Le Bozec, French Corrosion Institute

In this article, the authors describe the third and final part of a study that involved testing three paint systems over UHP waterjetted panels coated with a zinc-rich shop primer and compared the results to conventional grit blasttreated, similarly shop-primed panels....
(Login to read the full article)

   

Tagged categories: Construction; Shop-applied coatings; Steel; Surface Preparation; UHP waterjetting

Comment Join the Conversation:

Sign in to our community to add your comments.

Advertisements
 
Tarps manufacturing, Inc.

 
NLB Corporation

 
HoldTight Solutions Inc.

 
Modern Safety Techniques

 
Strand’s Industrial Coatings

 
CRW

 
Paint BidTracker

 
Sauereisen, Inc.

 
 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us