Laboratory Testing of Candidate Coating Systems for Protecting A 490 Bolts in One World Trade Center Construction

From JPCL, March 2010

by John Bullard, Port Authority of New York & New Jersey, and William D. Corbett, KTA-Tator, Inc.

In this article, the authors report on the surface preparation and coating system selection for the bolt/washer/nut assemblies for the new construction of One World Trade Center in New York. The article describes the methods of surface preparation and retreatments used, the coating systems selected and applied, the testing methodology, and the test results....
(Login to read the full article)

   

Tagged categories: Adhesion; ASTM; Coating Materials; Corrosion resistance; Galvanized steel; Laboratory testing; Research; Surface preparation; Surface Preparation

Comment Join the Conversation:

Sign in to our community to add your comments.

Advertisements
 
SAFE Systems, Inc.

 
DeFelsko Corporation

 
KTA-Tator, Inc. - Corporate Office

 
Tarps manufacturing, Inc.

 
AWWA (American Water Works Association)

 
Sauereisen, Inc.

 
Fischer Technology Inc.

 
 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us