New Waterborne Fluoropolymer Resins for Ultra-Weatherable Coatings

From JPCL, December 2009

by Winn Darden and Bob Parker, AGC Chemicals Americas; and Naoko Sumi, Isao Kimura, Masakazu Ataku, and Takashige Maekawa, Asahi Glass Co. Ltd.

this article describes solvent-borne and waterborne FEVE resins as well as the potential uses of new FEVE dispersion resins in coatings for field application where high weathering properties are needed....
(Login to read the full article)

   

Tagged categories: Accelerated laboratory testing; Coating Materials; FEVE; Fluoropolymer; Fluorourethane; Performance testing; Resins; Solventborne coatings; Waterborne coatings; Weathering

Comment Join the Conversation:

Sign in to our community to add your comments.

Advertisements
 
Tarps manufacturing, Inc.

 
Modern Safety Techniques

 
CRW

 
HoldTight Solutions Inc.

 
Paint BidTracker

 
Sauereisen, Inc.

 
Strand’s Industrial Coatings

 
 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us