Maintenance Tip: Evaluating Techniques for Measuring Applied Film Thickness of Polyurea Elastomeric Systems

From JPCL, March 2009

by Dudley J. Primeaux II, Primeaux Associates LLC, Elgin, TX and Kelin Bower, PolyVers Internatioanl, Houston, TX

In any coating or lining work, obtaining the specified minimum film thickness or the minimum average film thickness is essential....
(Login to read the full article)

   

Tagged categories: Applied film thickness; Coating / Film thickness; Concrete; Dry Film Thickness (DFT); Elastomeric coatings; Magnetic thickness gauge; Polyurea; Quality control; Ultrasonic thickness gauge; Wet film thickness; Wet film thickness gauge

Comment Join the Conversation:

Sign in to our community to add your comments.

Advertisements
 
NLB Corporation

 
HoldTight Solutions Inc.

 
Strand’s Industrial Coatings

 
EDCO - Equipment Development Co. Inc.

 
CRW

 
REMA Corrosion Control

 
Tarps manufacturing, Inc.

 
 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us