Investigating Corrosion Protection of Offshore Wind Towers

From JPCL, April 2008

by Andreas W. Momber, Ph.D., Muehlhan AG; Peter Plagemann, Ph.D., and Volkmar Stenzel, Ph.D., Fraunhofer Institute for Manufacturing and Applied Materials Research; and Michael Schneider, Ph.D., Fraunhofer Institute for Ceramic Technologies and Systems

In the first of a two-part article, the authors describe a funded project on performance testing of corrosion protection of wind energy mills, particularly the mill's steel tower and parts of the mill foundation. The article examines stressors of these structures (particularly corrosive stress) and details the selection of corrosion protection systems and the text procedures developed to evaluate them....
(Login to read the full article)

   

Comment Join the Conversation:

Sign in to our community to add your comments.

Advertisements
 
Axxiom Manufacturing

 
Western Technology Inc.

 
Sauereisen, Inc.

 
KTA-Tator, Inc. - Corporate Office

 
HoldTight Solutions Inc.

 
 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us