Mitigating Moisture in Concrete and
Masonry Walls

A Guide to Coatings, Water Repellents and Sealants

From JPCL, June 2016

By Kenneth A. Trimber and Kevin J. Brown, KTA-Tator Inc.

Mold, spalling and peeling coatings are some of the consequences of uncontrolled moisture intrusion into masonry and concrete walls. Learn how to select the best coatings, water repellents and sealants and identify the brand names of candidate materials and systems....


(Login to read the full article)
   

Tagged categories: Coating failure; concrete; Concrete coatings and treatments; Failure analysis; Good Technical Practice; Kenneth A. Trimber; KTA-Tator; Masonry; Moisture detection; Sealant; Waterproofing

Comment Join the Conversation:

Sign in to our community to add your comments.

Advertisements
 
KTA-Tator, Inc. - Corporate Office

 
Fischer Technology Inc.

 
Mitsubishi Gas Chemical America

 
Sauereisen, Inc.

 
SABRE Autonomous Solutions

 
NLB Corporation

 
DeFelsko Corporation

 
Modern Safety Techniques

 
RCG America

 
SAFE Systems, Inc.

 
 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us