D+D Print June 2014

 
D+D Print June 2014


View the Digital Edition of this Issue

Color + Design

Color Matters

by Jill Pilaroscia, Colour Studio Inc.

Whether by rebranding a property or helping to speed rentals, good color adds value.


Maintenance + Renovation

Vegetative Roof Durability: Lessons from Sandy

by Matthew Barmore, Firestone Building Products, and Elaine Kearney, Columbia Green Technologies

Two New Jersey case studies suggest that established plantings can survive even hurricane-force winds.


Coatings A to Zielnik

Fighting Fire with Fire Protectives

by Allen Zielnik, Atlas Material Testing Technology LLC

Modern intumescents have advanced significantly in both fire performance and aesthetics.


D+D Conference

Technology, Ideas Frame First-Ever D+D Conference and Exhibition

by Gary Henry

Historic hotel hosts design, construction conference.


Concrete Q + A

Breaking the Repair-Repeat Cycle

by Fred Goodwin, FICRI, FACI, BASF Construction Chemicals

A new repair code helps concrete deliver on its promise of long life.


Plus...


News

Architecture students reimagine an icon


Picture This!

The Color of Glass


Case Study

Profiles in Polyurea

by Gary Henry

Here’s a look at a few projects using this versatile polymer technology.


Perspective

Lessons from Madge

by Gina R. Johnson, Editor in Chief


Materials Technology

Product Showcase: AIA Convention 2014

Preview from the exhibit hall


Clues to a Coating Failure

Avoiding Fading Paint

by Jayson L. Helsel, P.E., KTA-Tator Inc.

Uneven paint at a retail store offers lessons for specifying high-performance paint.


   
Advertisements
 
DeFelsko Corporation

 
KTA-Tator, Inc. - Corporate Office

 
SAFE Systems, Inc.

 
WEFTEC Show

 
Tarps manufacturing, Inc.

 
Sauereisen, Inc.

 
 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us