True or false: The anhydrous calcium chloride test can measure the level of salt contamination on concrete substrates.


What is the name of a rigid cell used to collect soluble salts from a contaminated surface to determine the concentration of the salt?


What is the name of a rigid cell used to determine soluble salt concentrations on steel?


What is the name of the test for measuring soluble salt concentrations on steel surfaces prior to painting by applying a special patch to the substrate, injecting deionized water beneath it, and then extracting the water to measure its conductivity?


What instrument would you use to analyze soluble salt contamination on abrasives?


True or False: Maximum levels of soluble salts that can remain on a steel substrate after surface preparation are mandated in SSPC-Guide 15 and ISO 8502.


Which of the following is a recognized method for removing soluble salts from a steel substrate to test concentration levels?


 
 
   

**Commercial white papers, product videos, and other sponsored documents posted on this site are paid content from third-party companies; inclusion and posting on this site does not imply an endorsement nor recommendation of the content by Technology Publishing/PaintSquare. By signing in and viewing or downloading this paid content, you agree to make your name and full contact information available to the sponsor of the content.

Advertisements
 
SAFE Systems, Inc.
 
Portable Blast &
Recovery Equipment
 
Trailer or skid mounted blast and recovery equipment. Systems designed for maximum versatility, environmental compliance
and overall cost savings.
Call 1-800-634-7278
 

 
Tarps manufacturing, Inc.
 
QUALITY MADE IN AMERICA —Available near you!
 
CLICK to get a behind-the-scenes look at how Tarps Manufacturing makes the highest-quality tarps right here in the USA — available nationwide.
 

 
SEMicro Division, M.E. Taylor Engineering, Inc.
 
Coatings Adhesion Testers
 
The PATTI® accurately measures the bond strength between coating & substrate. Outfitted properly, the surface can be rough, porous, or curved & >10K psi strong!
 

 
Industrial Vacuum Equipment Corp.
 
Hurricane Vacuums
& Dust Collectors
 
Vacuum and dust collector hose, filters and related accessories.
IndustrialVacuum.com
 

 
HoldTight Solutions Inc.
 
NO FLASH RUST - NO CONTAMINANTS
 
Our HoldTight®102 salt remover & flash rust
preventer prevents flash
rust by removing surface contaminants. Contact us
for your nearest distributor.
(800) 319.8802 sales@holdtight.com
 

 
CHLOR*RID International Inc.
 
SOLUTIONS THAT WORK
 
Companies that invest in corrosion control use CHLOR RID products
  • Soluble salt removal liquid
  • Test kits to verify contamination levels
  • Surface passivation to hold the blast
INFO@CHLOR-RID.COM 800.422.3217
 

 
Sauereisen, Inc.
 
SewerGard® 210XHB
 
• 300 mils in a single coat by plural component equipment
• Fast Setting
• 100% Solids Epoxy
• Chemical-resistant barrier for municipal wastewater environments
sauereisen.com
 

 
ABKaelin, LLC
 
ABKAELIN EH&S SERVICES
 
Programs/Training/Monitoring for Silica, Lead, Noise, Beryllium, Hexavalent Chromium, Cadmium, Hazardous Waste*PM10 & TSP-Lead Ambient Air Monitoring*SSPC C3/C5
 

 
Fischer Technology Inc.
 
Maximize Profits by Monitoring Coating Thickness
 
Learn more by contacting Fischer Technology today: 1.860.683.0781
 

 
Monti Tools, Inc.
 
BRISTLE BLASTER® – THE ORIGINAL ONE
 
  • Abrasive blast with a power tool
  • Remove corrosion, mill scale and coatings
  • Cleans & roughens
  • Meets SSPC-SP 10 / NACE No. 2
  • Profile up to 4.7 mils
  • ATEX Zone 1
  •  

     

    Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

    TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


    The Technology Publishing Network

    Durability + Design PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

     
    EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
    REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
    MORE:      About PaintSquare.com   |   Privacy policy (Updated 1/8/2018)   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us