SSPC-TR 5/ICRI 03741/NACE 02203, Design, Installation, and Maintenance of Protective Polymer Flooring Systems for Concrete

All Standards | SSPC Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date: November 01, 2003
Updated On: November 01, 2003
Editorial Change:
 
This technical committee report provides information on the design, installation, and maintenance of protective polymer flooring systems that are applied and directly bonded to concrete.

This report focuses on those aspects of design, materials, and installation procedures that can help the user attain long-term service from a variety of polymer flooring systems for a wide range of applications.

This report is intended for use by manufacturers, specifiers, applicators, and facility owners who specify protective polymer flooring systems for concrete.

(Back to all Standards)

 
   

Bayer MaterialScience LLC
Desmodur® XP 2763 Drives Financial Results

High performance polyaspartic coatings
• Dry faster
• Fewer coats
• Superior corrosion/weather resistance
412-777-3983


Industrial Vacuum Equipment Corp.
Hurricane Vacuums
& Dust Collectors

Vacuum and dust collector hose, filters and related accessories.
IndustrialVacuum.com


Cardolite Corporation
CNSL Based Products

Renewable CNSL epoxy curing agents and resins with fast cure at low temperature, adhesion to unprepared surfaces and excellent corrosion and water protection.


MSA (The Safety Company)
Free Whitepaper: A Quick Guide to Air-Purifying Respirators

Download a whitepaper on air-purifying respirators and powered air-purifying respirators from the safety experts at MSA.


Blastox/The TDJ Group, Inc.
Blastox - One Step
Lead Abatement

Don't waste $$ on added labor steps with other methods. Don't mix, meter or apply at the job-site. Avoid strict hazardous waste rules.
Let your painters paint!


Van Air Systems
The Blast Pak

Van Air Systems' portable desiccant air dryer. Get dry compressed air with this All-In-One blasting and coating solution.


Hempel (USA) Inc.
Real Coating
for Real Protection

Hempel's protective coatings cover a wide range of applications across multiple industries from oil and gas to power generation to infrastructure.

 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker JPCL Europe

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2013, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com