NACE No. 10/SSPC-PA 6 NACE No. 10/SSPC-PA 6 Fiberglass-Reinforced Plastic (FRP) Linings Applied to Bottoms of Carbon Steel Aboveground Storage Tanks

All Standards | NACE Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date:
Updated On: July 18, 2012
Editorial Change:
 
New in 2002! This standard recommended practice specifies the procedures to design, apply, and inspect fiberglass reinforced plastic (FRP) linings that are applied internally to the bottom of carbon steel aboveground storage tanks (ASTs). This recommended practice will serve as a resource to facility owners preparing specifications for achieving successful lining applications in ASTs in the petroleum/petrochemical industry. However, the practices described are useful during preparation of specifications for ASTs in other services as well.

(Back to all Standards)

 
   

GMA Garnet USA
GMA Garnet™
Natural Abrasives

- Superior cleaning performance
- Even Profile
- Low Dust
- Cost-Effective
- Environmentally friendly
- Recyclable up to 5 times
Tel : +1 832 243 9300


STOPAQ
Click here if you
Dare to Compare

Permanent Visco-Elastic Corrosion Prevention Traditional systems versus Stopaq Solutions.


Van Air Systems
Need Dry
Compressed Air?

Van Air Systems' Blast Pak is the answer! The Blast Pak is a drying package that leaves contractors with cool, clean and dry compressed air, Ideal for mobile blasting & painting contractors.


Atlantic Design, Inc.
We’ve Got a Surprise For You!

We’ve designed two new lines
of equipment with shorter lead
times, budget friendly prices,
more safety features & all
with the same ADI quality!
866.Call.ADI


No Ordinary Soda
ARMEX® baking soda-based abrasives from the makers of ARM & HAMMER® products offers over 12 formulas specially engineered for your application and your budget.


Industrial Vacuum Equipment Corp.
Hurricane Vacuums
& Dust Collectors

Vacuum and dust collector hose, filters and related accessories.
IndustrialVacuum.com


U.S. Zinc

www.USZINC.com


Combat deterioration and
corrosion with our zinc
dust in your paints and
coatings. U.S. Zinc helps
the world work.

 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker JPCL Europe

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2013, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com