D5162 Standard Practice for Discontinuity (Holiday) Testing of Nonconductive Protective Coating on Metallic Substrates

All Standards | ASTM Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date:
Updated On: July 29, 2008
Editorial Change:
 
1.1 This practice covers procedures for determining discontinuities using two types of test equipment: 1.1.1 Test Method A—Low Voltage Wet Sponge, and 1.1.2 Test Method B—High Voltage Spark Testers.

1.2 This practice addresses metallic substrates. For concrete surfaces, refer to Practice D 4787.

1.3 The values stated in SI units are to re regarded as the standard. The values given in parentheses immediately following the metric units are for information only.

1.4 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.

(Back to all Standards)

 
   

Clemco Industries Corp.
Powerful Protection in a Small Package

Mounts inside blast helmet, alerts operator to dangerous breathing-air condition by audible, visual, and vibratory alarms. Easily calibrated, battery operated.


CHLOR*RID International Inc.
Surface cleanliness is
ESSENTIAL to coating
performance.

* TEST FOR SALTS
* PREVENT FLASH RUST
* REMOVE SALTS
More information at
www.chlor-rid.com,

800-422-3217


Fischer Technology Inc.
Gauges Meet IMO-PSPC & SSPC-PA2 Requirements

• USB or optional Bluetooth
• Custom inspection reports
• Excellent on edges & rough surfaces; Optimum accuracy
• Largest selection of probes to meet challenging situations
Call Fischer: 800-243-8417


BASF
New resins from BASF will have metals loving water:

Excellent corrosion resistance, low VOC, high gloss, thin films basf.us/industrialcoatings
polyorders@basf.com
800-231-7868


Fox Industries Inc.
Repair, Protect & Strengthen

Need a coating? Turn to Fox. We have solutions to repair, protect and strengthen concrete, steel and wood substrates. Call 888-760-0369 or email info@foxind.com


International Bridge Conference
International Bridge Conference

Join us in Pittsburgh over June 2-6, 2013 to celebrate the 30th Anniversary of the International Bridge Conference®, the world’s premier technical conference on bridges.


DRYCO
Climate Control...delivered.

Temporary climate control equipment. Dehumidifiers,
Heaters, A/C, Power, More…
Toll Free: 866-379-2600

 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker JPCL Europe

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2013, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com