SSPC-Paint 36, Two-Component Weatherable Aliphatic Polyurethane Topcoat, Performance-Based

All Standards | SSPC Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date: April 01, 2006
Updated On: April 01, 2002
Editorial Change: April 1, 2006
 
This specification covers the requirements for a high performance, two-component, UV-stable polyurethane topcoat (ASTM D 16, Type V polyurethane). It is intended for a topcoat that provides excellent color and gloss retention, not for thick section elastomeric coatings.

Coatings meeting the requirements of this specification are generally suitable for exposures in environmental zones 1A (interior, normally dry), 1B (exterior, normally dry), 2A (frequently wet by fresh water, excluding immersion), 2B (frequently wet by salt water, excluding immersion), 3B (chemical exposure, neutral), and 3C (chemical exposure, alkaline).

The specified coating is intended for application by brush, spray, or roller. It is generally applied over a primer or intermediate coating.

(Back to all Standards)

 
   

No Ordinary Soda
ARMEX® baking soda-based abrasives from the makers of ARM & HAMMER® products offers over 12 formulas specially engineered for your application and your budget.


SSPC: The Society for Protective Coatings
http://www.sspc.org/

Join SSPC and Enhance
Your Career !


MMLJ
Superfast Dustless Abrasive Blasting - Watch Video

Dustless Blasting creates no dust plume so others can work nearby unaffected. Maximize Productivity! Watch our numerous YouTube videos to learn more.


DRYCO
The one way to control
a tank: DRYCO

Temporary climate control equipment. Dehumidifiers,
Heaters, A/C, Power, More…
Toll Free: 866-379-2600


Absolute Equipment/Grand Rental Station
Portable Power from Absolute Equipment

•Compressors
•Lighting Systems
•Generators
•Light Compaction
Sales • Rental • Service
Call 1-866-931-6655
Over a century of
providing excellence.


SAFE Systems, Inc.
Enduroguard -
The Tough Cable
for a Tough Industry.

Reduce maintenance costs and down time, increase job site safety with Enduroguard Cable. Available exclusively from SAFE Systems. UL listed, flexible, abrasion resistant and cut resistant.


Termarust Technologies
Termarust (HR CSA) Chemically Stops
Active Corrosion

Truss bridge treated in 2000 with Termarust's (HR CSA) field-proven rust mitigation system chemically stopped corrosion, crevice corrosion & pack rust.

 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker JPCL Europe

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2013, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com