ISO 6957:1988 ISO 6957:1988 Copper alloys -- Ammonia test for stress corrosion resistance

All Standards | ISO Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date:
Updated On: April 01, 2002
Editorial Change:
 
Specifies a test, using an ammoniacal atmosphere, for the detection of applied or residual stresses which can cause failure of the material in service or storage through stress corrosion cracking. The severity of the method can be regulated by changing the pH value. In an informative annex, recommendations are given for the choice of pH-values.

(Back to all Standards)

 
   
Advertisements
 
Fischer Technology Inc.
 
DUALSCOPE®FMP100 with DataCenter IP
 
Transfer customized inspection plans from PC to FMP100 using step-by-step guidance with prompts and pictures throughout the measurement procedure
 

 
ABKaelin, LLC
 
ABKAELIN EH&S SERVICES
 
Programs/Training/Monitoring for Silica, Lead, Noise, Beryllium, Hexavalent Chromium, Cadmium, Hazardous Waste*PM10 & TSP-Lead Ambient Air Monitoring*SSPC C3/C5
 

 
HoldTight Solutions Inc.
 
NO FLASH RUST - NO CONTAMINANTS
 
Our HoldTight®102 salt remover & flash rust
preventer prevents flash
rust by removing surface contaminants. Contact us
for your nearest distributor.
(800) 319.8802 sales@holdtight.com
 

 
SABRE Autonomous Solutions
 
Productivity
 
Personnel are free to do other tasks while the ALPHA1 does the “dirty work”.
 

 
Industrial Vacuum Equipment Corp.
 
Hurricane Vacuums
& Dust Collectors
 
Vacuum and dust collector hose, filters and related accessories.
IndustrialVacuum.com
 

 
SAFE Systems, Inc.
 
Portable Blast &
Recovery Equipment
 
Trailer or skid mounted blast and recovery equipment. Systems designed for maximum versatility, environmental compliance
and overall cost savings.
Call 1-800-634-7278
 

 
KTA-Tator, Inc. - Corporate Office
 
New KTA Pipeline Inspection Kit
 
• Defelsko standard memory body
• Positector FTS 0-250 mils, cabled dry film thickness probe
• NEW Positector Shore D hardness probe
• All essential inspection equipment!
Visit www.ktagage.com
 

 
Carboline Company
 
New product: Carbozinc® 608 HB
 
Introducing a new high build zinc-rich primer that can save you time and money by eliminating the epoxy intermediate coat!
 

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

Durability + Design PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us