SSPC-Paint 30, Weld-Through Inorganic Zinc Primer

All Standards | SSPC Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date: April 01, 2002
Updated On: April 01, 2002
Editorial Change: November 1, 2004
 
This specification covers a group of inorganic zinc primers that can protect carbon steel during the fabrication process, permit welding to specification requirements, and be overcoated.

The major pigment component in this coating is zinc dust and the binder is inorganic

This specification defines the minimum compositional and laboratory performance requirements for characterizing a group of zinc primers. It is to be used in conjunction with SSPC-PS Guide 22.00, SSPC-PS Guide 12.00, and other SSPC specifications covering surface preparation, application, thickness, inspection, and safety.

(Back to all Standards)

 
   

GMA Garnet USA
GMA Garnet™
Natural Abrasives

- Superior cleaning performance
- Even Profile
- Low Dust
- Cost-Effective
- Environmentally friendly
- Recyclable up to 5 times
Tel : +1 832 243 9300


Modern Safety Techniques
Modern Safety Techniques

See our Low Temperature Catalyst for your CO removal needs. Help to provide your workers with safe, comfortable breathing air!


ANAFAPYT (Asociación Nacional de Fabricantes de Pinturas y Tintas)
ANAFAPYT Latin American
Coatings Show 2013

You are still on time to sign up
for Conferences, Exhibit Floor
and Short Course. Be part of
the best show in Latin
America. www.lacs2013.com


ElektroPhysik
High-precision coating thickness gauge MiniTest 7400

MiniTest 7400 with intuitive menu control, enhanced data management with configuration assistent. Wear-resistant sensors for measuring tasks up to 35mm thickness.


Termarust Technologies
Termarust (HR CSA) Chemically Stops
Active Corrosion

Truss bridge treated with Termarust's (HR CSA) in 1995. This highway & rail truss bridge is still stable and there still is no active corrosion.


STOPAQ
Click here if you
Dare to Compare

Permanent Visco-Elastic Corrosion Prevention Traditional systems versus Stopaq Solutions.


JPCL - PCE - PaintSquare
Charter Advertising Opportunities Available through April 30.

Click above or contact Bernadette Landon
Publisher, JPCL Europe blandon@jpcleurope.com +1.412.697.0184
visit www.jpcleurope.com

 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker JPCL Europe

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2013, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com