ISO 11127-3:2011 ISO 11127-3:2011 Preparation of steel substrates before application of paints and related products -- Test methods for non-metallic blast-cleaning abrasives -- Part 3: Determination of apparent density

All Standards | ISO Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date:
Updated On: August 01, 2012
Editorial Change:
 
The procedure includes drying a sufficient quantity of the sample by heating, allowing to cool to room temperature, adding distilled or deionized water to the cleaned, dried and weighed pyknometer containing 10 g of the dried sample until it is completely filled, displacing air adhering to the test portion, drying the outside of the pyknometer, reweighing the pyknometer and its contents, emptying the pyknometer, refilling with distilled or deionized water, drying the outside and weighing again.

(Back to all Standards)

 
   

Fischer Technology Inc.
Gauges Meet IMO-PSPC & SSPC-PA2 Requirements

• USB or optional Bluetooth
• Custom inspection reports
• Excellent on edges & rough surfaces; Optimum accuracy
• Largest selection of probes to meet challenging situations
Call Fischer: 800-243-8417


Madison Chemical Industries Inc.
There’s only one CorroCote

Madison invented CorroCote
in 1974 to prevent corrosion
in underground fuel storage
tanks. Today, it’s still the
classic coating for protecting
infrastructure


SAFE Systems, Inc.
Portable Dust Collectors for Tough Environments

Trailer and skid-mounted models in numerous sizes, powered by electric and/or diesel. Sloped roofs, multiple dust inlets, high static, dampered fans. Lockable power & drive compartments.


Denso North America Inc.
Tank Base Protection

An easy to apply system utilizing Denso tapes and coatings around the tank base, that helps prevent corrosion from external elements.
Call 1-281-821-3355 or Visit densona.com


Safway Services
One Source. Every Solution.

The Safway Group is your source for multiservices. Painting, coating, insulation and more – all from the most trusted name in the industry.


NLB Corporation
Handheld VertaJet™ for concrete or steel

Ergonomic VertaJet from NLB boosts surface prep productivity. Rotating 40,000 psi water jets strip a 6” path and get into corners, with vacuum recovery.


MSA (The Safety Company)
Free Whitepaper: A Quick Guide to Air-Purifying Respirators

Download a whitepaper on air-purifying respirators and powered air-purifying respirators from the safety experts at MSA.

 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker JPCL Europe

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2013, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com