ISO 11124-4:1993 Preparation of steel substrates before application of paints and related products -- Specifications for metallic blast-cleaning abrasives -- Part 4: Low-carbon cast-steel shot

All Standards | ISO Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date:
Updated On: April 01, 2002
Editorial Change:
 
Specifies requirements for 12 grades of low-carbon cast-steel shot abrasive: designation, sampling, package identification and lot traceability, information to be supplied by the manufacturer or supplier, hardness, density, defect/structural requirements and chemical composition. The requirements specified apply to abrasives supplied in the "new" condition only.

(Back to all Standards)

 
   

Montipower, Inc.
The MBX Bristle Blaster

Get a 2.7 to 3.3 mil profile and a Near White Metal Clean. For info visit www.mbxit.com or call 877 629-8777


Corrosion Specialties, Inc.
The T93R Airless
Tip System

is the longest lasting, highest quality tip and guard available to coatings applicators around the world. Click the link to contact Corrosion Specialties.


Madison Chemical Industries Inc.
Your zinc-rich primer
is obsolete!

Madison’s Zinc-Rich
technology takes the
state of the art to a
new level. AlumiZinc ‘S’
offers superior protection
in a user-friendly
and forgiving format.


Wasser High-Tech Coatings Inc.
Wasser Coatings

have been used to protect some of the most important bridges in the country; learn about our NEPCOAT-approved system as well as our entire range of MCU coatings and Polyurea membranes.


BASF
New resins from BASF will have metals loving water:

Excellent corrosion resistance, low VOC, high gloss, thin films basf.us/industrialcoatings
polyorders@basf.com
800-231-7868


Modern Safety Techniques
Modern Safety Techniques

With our unique LTCat, we can help to provide clean, safe breathing air to your workers. Take a look at our Breathing Air Systems, we supply at least twice as much charcoal as our competitors! Modern


Harsco
BLACK BEAUTY® GLASS

A 100% post-consumer bottle glass abrasive from a company you can trust. Toll Free: 1-888-733-3646

 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker JPCL Europe

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2013, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com