ISO 8502-6:2006 ISO 8502-6:2006 Preparation of steel substrates before application of paints and related products -- Tests for the assessment of surface cleanliness -- Part 6: Extraction of soluble contaminants for analysis -- The Bresle method

All Standards | ISO Standards
Search Standards

Click to Purchase and Download this Standard or Test Method

Revision Date:
Updated On: August 04, 2012
Editorial Change:
Describes a method of extraction, intended for analysis, of soluble contaminants from a surface by means of adhesive patches which can be attached to any surface, regardless of its shape and orientation. Suitable for use in the field before application of paints.

(Back to all Standards)

SABRE Autonomous Solutions
Personnel are free to do other tasks while the ALPHA1 does the “dirty work”.

New resins from BASF will have metals loving water!
Excellent corrosion resistance, low VOC, high gloss, thin films 800-231-7868

DeFelsko Corporation
PosiTector SST Soluble Salt Tester
Measures the concentration of soluble salts on metal surfaces. Use with all Bresle patch types including the reusable, adhesive-free PosiPatch.

Fischer Technology Inc.
DUALSCOPE®FMP100 with DataCenter IP
Transfer customized inspection plans from PC to FMP100 using step-by-step guidance with prompts and pictures throughout the measurement procedure

ABKaelin, LLC
Programs/Training/Monitoring for Silica, Lead, Noise, Beryllium, Hexavalent Chromium, Cadmium, Hazardous Waste*PM10 & TSP-Lead Ambient Air Monitoring*SSPC C3/C5

SAFE Systems, Inc.
Portable Dust Collectors for Tough Environments
Trailer and skid-mounted models in numerous sizes, powered by electric and/or diesel. Sloped roofs, multiple dust inlets, high static, dampered fans. Lockable power & drive compartments.

CHLOR*RID International Inc.
Companies that invest in corrosion control use CHLOR RID products
  • Soluble salt removal liquid
  • Test kits to verify contamination levels
  • Surface passivation to hold the blast
INFO@CHLOR-RID.COM 800.422.3217

Sika® Industrial Floor Coatings
Click to learn about floor and wall systems relied upon for performance, durability, easy maintenance and aesthetics across the every industry and environment.

HoldTight Solutions Inc.
Our HoldTight®102 salt remover & flash rust
preventer prevents flash
rust by removing surface contaminants. Contact us
for your nearest distributor.
(800) 319.8802


Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL

The Technology Publishing Network

Durability + Design PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us