ISO 8781-3:1990 ISO 8781-3:1990 Pigments and extenders -- Methods of assessment of dispersion characteristics -- Part 3: Assessment from the change in gloss

All Standards | ISO Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date:
Updated On: April 01, 2002
Editorial Change:
 
The method is of general use for comparing similar pigments, for example a test pigment against an agreed reference pigment. The pigment is dispersed in stages under specified conditions in an agreed binder system. After each stage, a portion of the mill base is taken and made into a composition that is applied to a substrate and dried or stoved.

(Back to all Standards)

 
   

ElektroPhysik
High-precision coating thickness gauge MiniTest 7400

MiniTest 7400 with intuitive menu control, enhanced data management with configuration assistent. Wear-resistant sensors for measuring tasks up to 35mm thickness.


U.S. Zinc

www.USZINC.com


Combat deterioration and
corrosion with our zinc
dust in your paints and
coatings. U.S. Zinc helps
the world work.


Abrasives Inc.
One Call Orders it All!

Life is good when it’s simple. We distribute Clemco blast equipment, nozzles & parts alongside our proven blast media. Make your call: Abrasives Inc. 800-584-7524


Modern Safety Techniques
Modern Safety Techniques

With our unique LTCat, we can help to provide clean, safe breathing air to your workers. Take a look at our Breathing Air Systems, we supply at least twice as much charcoal as our competitors! Modern


Safway Services
One Source. Every Solution.

The Safway Group is your source for multiservices. Painting, coating, insulation and more – all from the most trusted name in the industry.


Clemco Industries Corp.
Powerful Protection in a Small Package

Mounts inside blast helmet, alerts operator to dangerous breathing-air condition by audible, visual, and vibratory alarms. Easily calibrated, battery operated.


Harsco
BLACK BEAUTY® GLASS

A 100% post-consumer bottle glass abrasive from a company you can trust. Toll Free: 1-888-733-3646

 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker JPCL Europe

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2013, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com