ISO 787-19:1974 ISO 787-19:1974 General methods of test for pigments -- Part 19: Determination of water-soluble nitrates (Salicylic acid method)

All Standards | ISO Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date:
Updated On: April 01, 2002
Editorial Change:
 
This document specifies a spectrophotometric method. The principle of the method consists in that the nitrate present in the extract of the sample is used to nitrate salicylic acid in sulphuric acid medium.

(Back to all Standards)

 
   

Versaflex Inc.
Best NSF 61.5 Approved Potable Water Polyurea

VersaFlex Polyurea Earns Highest ANSI/NSF 61.5 Rating for High Temp Service, Minimum Tank Size and Max Thickness. All Polyureas Are Not Created Equal. FREE WHITE PAPER.


JPCL - PCE - PaintSquare
Charter Advertising Opportunities Still Available

Click above or contact Bernadette Landon
Publisher, JPCL Europe blandon@jpcleurope.com +1.412.697.0184
visit www.jpcleurope.com


Safway Services
One Source. Every Solution.

The Safway Group is your source for multiservices. Painting, coating, insulation and more – all from the most trusted name in the industry.


Dow Corning Corporation
New Dow Corning® 3055 Resin

Ensure long-term asset protection and extend repaint cycles with a low-VOC, two-coat polysiloxane coating featuring superior corrosion and moisture resistance.


Industrial Vacuum Equipment Corp.
Hurricane Vacuums
& Dust Collectors

Vacuum and dust collector hose, filters and related accessories.
IndustrialVacuum.com


Corrosion Probe, Inc.
From Detection to Correction

Corrosion Probe, Inc. has the Most Concrete Coatings Experience and Expertise. Contact us today at
860-767-4402, www.cpiengineering.com


EDCO - Equipment Development Co. Inc.
We are American Made

Visit all of EDCO’s Internet homes:
EDCOINC.com
ContrxSystems.com
EDCOFabrication.com
YouTube Channel–search
EDCOincorporated
EDCO Twitter: @EDCOUSA 800-638-3326

 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker JPCL Europe

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2013, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com