ISO 7724-2:1984 ISO 7724-2:1984 Paints and varnishes -- Colorimetry -- Part 2: Colour measurement

All Standards | ISO Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date:
Updated On: April 01, 2002
Editorial Change:
 
Describes the method for determining the colour co-ordinates of paint films. The method is only application to paint films that appear to be uniformly of one colour (monochromatic), when examined with normal vision.

(Back to all Standards)

 
   

Safety Lamp of Houston, Inc.
Wet & hazardous area lighting solutions from SAFETY LAMP of Houston

New WOLF LED and fluorescent lights are now available, including low voltage tank lighting kits.
Call: (281) 964-1019.


Bayer MaterialScience LLC
Desmodur® XP 2763 Drives Financial Results

High performance polyaspartic coatings
• Dry faster
• Fewer coats
• Superior corrosion/weather resistance
412-777-3983


Carboline Company
Hyrdrocarbon Fire & Jet Fire Protection

Pyroclad X1 is the latest breakthrough in epoxy based intumescent fireproofing technology


GMA Garnet USA
GMA Garnet™
Natural Abrasives

- Superior cleaning performance
- Even Profile
- Low Dust
- Cost-Effective
- Environmentally friendly
- Recyclable up to 5 times
Tel : +1 832 243 9300


Fischer Technology Inc.
Gauges Meet IMO-PSPC & SSPC-PA2 Requirements

• USB or optional Bluetooth
• Custom inspection reports
• Excellent on edges & rough surfaces; Optimum accuracy
• Largest selection of probes to meet challenging situations
Call Fischer: 800-243-8417


Denso North America Inc.
Tank Base Protection

An easy to apply system utilizing Denso tapes and coatings around the tank base, that helps prevent corrosion from external elements.
Call 1-281-821-3355 or Visit densona.com


Rapid Prep, LLC
Nation Wide Equipment Rentals

Rapid Prep, LLC is a full service provider of sandblasting & all other surface preparation equipment, with 60 years of experience within the industrial painting industry.

 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker JPCL Europe

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2013, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com