TM0294-2007 Testing of Embeddable Impressed Current Anodes for Use in Cathodic Protection of Atmospherically Exposed Steel-Reinforced Concrete

All Standards | NACE Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date:
Updated On: July 24, 2012
Editorial Change:
 
Revised in 2007. Provides users and manufacturers of embeddable anodes with a test method for evaluating the anode material to an expected lifetime criterion. It is applicable to embeddable anode materials, such as titanium mesh, commonly used for cathodic protection of atmospherically exposed steel-reinforced concrete. The test is intended to evaluate whether an embeddable anode material complies with minimum required specifications of design life expectancy at rated current output. This test method is not applicable to surface-mounted anodes or conductive coating materials.

(Back to all Standards)

 
   

Madison Chemical Industries Inc.
Coat steel without blasting

Madison’s No-Blast technology
eliminates the need for
abrasive blasting in a number
of service applications.
See it in action at
MadisonChemical.com.


Green Diamond Sand Products
Green Diamond is the “Chosen”one.

Your  source for  high quality specialty sand. Superior Blasting Efficiency and an Excellent Surface profile. Available for on-site assistance.


HoldTight Solutions Inc.
NO FLASH RUST -
NO CONTAMINANTS

Our HoldTight®102 salt remover & flash rush inhibitor prevents flash rust by removing surface contaminants.
Contact us for your nearest distributor. (800) 319.8802 sales@holdtight.com


Versaflex Inc.
Best NSF 61.5 Approved Potable Water Polyurea

VersaFlex Polyurea Earns Highest ANSI/NSF 61.5 Rating for High Temp Service, Minimum Tank Size and Max Thickness. All Polyureas Are Not Created Equal. FREE WHITE PAPER.


DRYCO
Environmental Controls
Equipment & Service

Temporary climate control equipment. Dehumidifiers,
Heaters, A/C, Power, More…
Toll Free: 866-379-2600


Axxiom Manufacturing
Schmidt Improves
Portable Blasters

Schmidt's VBS System reduces blowdown intensity, prevents exhaust from damaging floor while using no screens or filters. Reduces sound; Increasing safety.
Call 1-800-231-2085


BASF
New resins from BASF will have metals loving water:

Excellent corrosion resistance, low VOC, high gloss, thin films basf.us/industrialcoatings
polyorders@basf.com
800-231-7868

 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker JPCL Europe

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2013, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com