TM0193-2000 Laboratory Corrosion Testing of Metals in Static Chemical Cleaning Solutions at Temperatures Below 93°C (200°F)

All Standards | NACE Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date:
Updated On: July 24, 2012
Editorial Change:
 
Revised in 2000! Describes a simple method for measuring the relative corrosiveness of inhibited solutions used for chemical cleaning in a static system; the tests described are conducted with corrosion coupons in a clean solution. Addresses testing parameters not covered in ASTM D 3263, specifically surface-to-volume ratio, inhibitor handling, pitting corrosion, and the reporting procedure.

(Back to all Standards)

 
   

Van Air Systems
Need a Dry-O-Lite Refill?

Order Dry-O-Lite desiccant from Van Air Systems.
The dependable, and cost-effective solution for dry compressed air.


DeHumidification Technologies
HUMIDITY PROBLEMS?

DH Tech has the most innovative and reliable equipment available to
control humidity efficiently
and effectively.
IT'S UNDER CONTROL!


Dow Corning Corporation
New Dow Corning® 3055 Resin

Ensure long-term asset protection and extend repaint cycles with a low-VOC, two-coat polysiloxane coating featuring superior corrosion and moisture resistance.


CHLOR*RID International Inc.
Surface cleanliness is
ESSENTIAL to coating
performance.

* TEST FOR SALTS
* PREVENT FLASH RUST
* REMOVE SALTS
More information at
www.chlor-rid.com,

800-422-3217


GMA Garnet USA
GMA Garnet™
Natural Abrasives

- Superior cleaning performance
- Even Profile
- Low Dust
- Cost-Effective
- Environmentally friendly
- Recyclable up to 5 times
Tel : +1 832 243 9300


Green Diamond Sand Products
Green Diamond is the “Chosen”one.

Your  source for  high quality specialty sand. Superior Blasting Efficiency and an Excellent Surface profile. Available for on-site assistance.


Polyval Coatings
POLYFLEX brand Polyurea

high chemical resistant membranes are used extensively to protect our environment in secondary containment applications.

 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker JPCL Europe

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2013, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com