TM0172-2001 TM0172-2001 Determining Corrosive Properties of Cargoes in Petroleum Product Pipelines

All Standards | NACE Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date:
Updated On: July 24, 2012
Editorial Change:
 
Revised in 2001. Provides a uniform method of testing the corrosive properties of petroleum product pipeline cargoes. This standard provides guidelines for performing the test method described in ASTM D 665, modified so that it is applicable to gasoline and other petroleum products, and so that it permits analysis within a single working day. This short test is particularly applicable to a batch control procedure because of the need for prompt release of cargoes and because time is limited during the working day.

(Back to all Standards)

 
   

Cardolite Corporation
CNSL Based Products

Renewable CNSL epoxy curing agents and resins with fast cure at low temperature, adhesion to unprepared surfaces and excellent corrosion and water protection.


Bullard

The Next Generation
of Blasting

• Lighest
• Coolest
• Most Comfortable
• Most Dependable


Rapid Prep, LLC
Nation Wide Equipment Rentals

Rapid Prep, LLC is a full service provider of sandblasting & all other surface preparation equipment, with 60 years of experience within the industrial painting industry.


LS Industries
LS Blasters: Optimum Steel Cleaning Efficiency

Simplify surface prep with the precise shot control of LS Blasters. Our blast technology delivers optimum coverage and finish. 800-533-8008


Polyval Coatings
POLYFLEX brand Polyurea

high chemical resistant membranes are used extensively to protect our environment in secondary containment applications.


GMA Garnet USA
GMA Garnet™
Natural Abrasives

- Superior cleaning performance
- Even Profile
- Low Dust
- Cost-Effective
- Environmentally friendly
- Recyclable up to 5 times
Tel : +1 832 243 9300


Madison Chemical Industries Inc.
Coat steel without blasting

Madison’s No-Blast technology
eliminates the need for
abrasive blasting in a number
of service applications.
See it in action at
MadisonChemical.com.

 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker JPCL Europe

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2013, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com