SSPC-PS 10.01, Hot-Applied Coal Tar Enamel Painting System

All Standards | SSPC Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date: November 01, 1982
Updated On: April 01, 2002
Editorial Change: November 1, 2004
 
This specification covers a hot-applied coal tar painting system for underground and underwater steel structures, consisting of a primer and two hot-applied coats.

This system is suitable for use on parts or structures exposed in Environmental Zones 2C (fresh water immersion), 3B (chemical exposure, neutral), and 3C (chemical exposure, alkaline). It has good abrasion resistance. It is also suitable for underground use. It must be used with discretion for immersion in corrosive chemicals since the coating is dissolved by some organic solvents and attacked by oxidizing solutions.

The coal tar enamel must be topcoated with coal tar emulsion when exposed to sunlight to prevent checking and alligatoring.

(Back to all Standards)

 
   

DeFelsko Corporation
NEW PosiTector
Inspection Kits

PosiTector 6000 Coating Thickness Gage easily converts to a surface profile gage, dew point meter or ultrasonic wall thickness gage with a simple probe change.


Denso North America Inc.
Tank Base Protection

An easy to apply system utilizing Denso tapes and coatings around the tank base, that helps prevent corrosion from external elements.
Call 1-281-821-3355 or Visit densona.com


Versaflex Inc.
Best NSF 61.5 Approved Potable Water Polyurea

VersaFlex Polyurea Earns Highest ANSI/NSF 61.5 Rating for High Temp Service, Minimum Tank Size and Max Thickness. All Polyureas Are Not Created Equal. FREE WHITE PAPER.


Empire Scaffold
Work with a scaffold company you can trust

Empire Scaffold is a full-service scaffold company providing specialized, on-site support for the life of the project, with products & experience to keep your projects up & running, safely.


ElektroPhysik
High-precision coating thickness gauge MiniTest 7400

MiniTest 7400 with intuitive menu control, enhanced data management with configuration assistent. Wear-resistant sensors for measuring tasks up to 35mm thickness.


International Bridge Conference
International Bridge Conference

Join us in Pittsburgh over June 2-6, 2013 to celebrate the 30th Anniversary of the International Bridge Conference®, the world’s premier technical conference on bridges.


Axxiom Manufacturing
Schmidt Improves
Portable Blasters

Schmidt's VBS System reduces blowdown intensity, prevents exhaust from damaging floor while using no screens or filters. Reduces sound; Increasing safety.
Call 1-800-231-2085

 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker JPCL Europe

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2013, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com