SP0296-2010 SP0296-2010 Guidelines for Detection, Repair, and Mitigation of Cracking of Existing Petroleum Refinery Pressure Vessels in Wet H2S Environments

All Standards | NACE Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date:
Updated On: July 18, 2012
Editorial Change:
 
Revised in 2004!! Intended to be a primary source of information on cracking in wet H2S petroleum refinery environments. Provides guidelines on detection, repair, and mitigation of cracking of existing carbon steel refinery pressure vessels, including columns, heat exchangers, drums, reboilers, separators, and more. In this standard, “wet H2S service” is defined as refinery process environments in which the concentration of H2S is 50 ppmw or greater in the aqueous phase. Thirteen tables show the frequency and severity of cracking as reported in a survey conducted on the topic. Examples of cracking are shown in photographs. Replaces RPO 296-2000.

(Back to all Standards)

 
   
Advertisements
 
KTA-Tator, Inc. - Corporate Office
 
New KTA Pipeline Inspection Kit
 
• Defelsko standard memory body
• Positector FTS 0-250 mils, cabled dry film thickness probe
• NEW Positector Shore D hardness probe
• All essential inspection equipment!
Visit www.ktagage.com
 

 
BASF
 
New resins from BASF will have metals loving water!
 
Excellent corrosion resistance, low VOC, high gloss, thin films www.basf.us/industrialcoatings dpsolutions@basf.com 800-231-7868
 

 
International Bridge Conference
 
Bridge conference 2018
 
Registration for the 2018 IBC is now open! Join us in June for the biggest and best IBC ever! View the Program, Workshops and Exhibitors by clicking in the banner.
 

 
North Dakota State University
 
Coatings Science Short Course – Registration Open
 
North Dakota State University, June 10 – 15, 2018. The course is designed for all levels of scientists and technologists working in the field of coating.
 

 
SAFE Systems, Inc.
 
Portable Blast &
Recovery Equipment
 
Trailer or skid mounted blast and recovery equipment. Systems designed for maximum versatility, environmental compliance
and overall cost savings.
Call 1-800-634-7278
 

 
Fischer Technology Inc.
 
Maximize Profits by Monitoring Coating Thickness
 
Learn more by contacting Fischer Technology today: 1.860.683.0781
 

 
Modern Safety Techniques
 
Modern Safety Techniques
 
With our unique LTCat, we can help to provide clean, safe breathing air to your workers. Take a look at our Breathing Air Systems, we supply at least twice as much charcoal as our competitors! Modern
 

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

Durability + Design PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us