RP0287-2002 RP0287-2002 Field Measurement of Surface Profile of Abrasive Blast Cleaned Steel Surfaces Using a Replica Tape

All Standards | NACE Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date: October 14, 2002
Updated On: July 18, 2012
Editorial Change:
 
Provides a procedure for measuring the surface profile of abrasive blast cleaned steel that involves using a special tape that replicates the surface profile. The standard covers the areas of equipment and procedures, provides a definition of "surface profile," and includes an appendix that presents the results of a round-robin series of measurements illustrating the degree of accuracy of the procedure described in the standard. A second appendix statistically summarizes the data presented in the first appendix.

(Back to all Standards)

 
   

International Bridge Conference
International Bridge Conference

Join us in Pittsburgh over June 2-6, 2013 to celebrate the 30th Anniversary of the International Bridge Conference®, the world’s premier technical conference on bridges.


DRYCO
The one way to control
a tank: DRYCO

Temporary climate control equipment. Dehumidifiers,
Heaters, A/C, Power, More…
Toll Free: 866-379-2600


Madison Chemical Industries Inc.
Coat steel without blasting

Madison’s No-Blast technology
eliminates the need for
abrasive blasting in a number
of service applications.
See it in action at
MadisonChemical.com.


EDCO - Equipment Development Co. Inc.
EDCO's Quick Response Codes

EDCO now includes Quick Response Code decals on machines. These QRC's provide customers with instant jobsite advice, problem solving tips and much more. Click to watch EDCO machines in action.


Greenhorne & O'Mara, Inc.
One Team. Infinite Solutions.

Greenhorne & O’Mara is now Stantec. Contact us for coatings and corrosion consulting, design, analysis, and inspection services at john.woods@stantec.com.


JPCL - PCE - PaintSquare
Charter Advertising Opportunities Available through April 30.

Click above or contact Bernadette Landon
Publisher, JPCL Europe blandon@jpcleurope.com +1.412.697.0184
visit www.jpcleurope.com


Dow Corning Corporation
New Dow Corning® 3055 Resin

Ensure long-term asset protection and extend repaint cycles with a low-VOC, two-coat polysiloxane coating featuring superior corrosion and moisture resistance.

 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker JPCL Europe

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2013, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com