D478 Standard Specification for Zinc Yellow (Zinc Chromate) Pigments

All Standards | ASTM Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date: August 09, 2012
Updated On: October 01, 2012
Editorial Change:
 
1.1 This specification covers the pigments commercially known as zinc yellow (zinc chromate).

1.2 Two types are included:

1.2.1 Type I -High-purity, low sulfate and chloride content.

1.2.2 Type II -Regular grade.

(Back to all Standards)

 
   
Advertisements
 
Fischer Technology Inc.
 
FISCHER Expands Corrosion Product Line
 
Rounding out Fischer’s extensive line of products for measuring protective coatings in the corrosion industry is the new ultrasonic wall thickness gauge UMP series.
 

 
CHLOR*RID International Inc.
 
SOLUTIONS THAT WORK
 
Companies that invest in corrosion control use CHLOR RID products
  • Soluble salt removal liquid
  • Test kits to verify contamination levels
  • Surface passivation to hold the blast
INFO@CHLOR-RID.COM 800.422.3217
 

 
DeFelsko Corporation
 
PosiTector SHD Shore Hardness Durometer
 
PosiTector SHD measures the hardness of non-metallic materials. Features a measurement timer, auto ignore mode and internal memory. Shore A or D available.
 

 
Blastox/The TDJ Group, Inc.
 
Blastox® - One Step Lead Abatement
 
Sandblast additive delivered to jobsite pre-blended to eliminate hazardous abrasive wastes. Why mix, meter or apply at the job-site? Blast with ease and
Let your painters paint!
1(800)-252-7869
 

 
US Minerals
 
Hit Harder. Clean Faster.
 
Black Diamond abrasive products are the toughest, most effective blasting media and supply the superior power you need to get any job done.
 

 
SABRE Autonomous Solutions
 
Quality
 
The ALPHA1 provides a consistent finish day-in
day-out; job to job.
 

 
HoldTight Solutions Inc.
 
NO FLASH RUST - NO CONTAMINANTS
 
Our HoldTight®102 salt remover & flash rust
preventer prevents flash
rust by removing surface contaminants. Contact us
for your nearest distributor.
(800) 319.8802 sales@holdtight.com
 

 
KTA-Tator, Inc. - Corporate Office
 
KTA-Tator EH&S Services
 
• Ambient & Worker Exposure Air Monitoring
• Safety & Health Program Development
• Lead Paint Assessments
& Specifications
• Health Hazard & Jobsite Safety Assessments
Call 1-800-532-3633
 

 
Vector Technologies Ltd.
 
The Original Performance Proven Vacuum Solutions
 
VecLoader® 616 Double Dump, Continuous Vacuum, 170 HP w/ 2,400 CFM & 28” Hg. 33% More Efficient than traditional vacuum systems! Choose Vector for the most powerful and the most reliable trailer mounted vacuums in the industry! Email us at: inquiry@vector-vacuums.com or call us at: 800-832-4010
 

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

Durability + Design PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us