D6237 Standard Guide for Painting Inspectors (Concrete and Masonry Substrates)

All Standards | ASTM Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date: March 30, 2009
Updated On: April 10, 2009
Editorial Change:
 
This guide is intended as a reference for those concerned with the inspection of thin- or thick-film coating application to concrete and masonry substrates. It does not cover the application of cement-type coatings. A checklist is included as Appendix X1.1. Many of the details covered may be in a specification for a particular project. A specification for coating projects should include the coatings to be used.

1.1 This guide is intended as an information aid to painting inspectors in carrying out the task efficiently. It includes the key elements of surface preparation, coatings application, and final approval for both field and shop work. The items should be selected that are pertinent to a particular job.

1.2 The values stated in SI units are to be regarded as the standard. The values given in parentheses are for information only.

1.3 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of whomever uses this standard to consult and establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.

(Back to all Standards)

 
   

Industrial Vacuum Equipment Corp.
Hurricane Vacuums
& Dust Collectors

Vacuum and dust collector hose, filters and related accessories.
IndustrialVacuum.com


DRYCO
The one way to control
a tank: DRYCO

Temporary climate control equipment. Dehumidifiers,
Heaters, A/C, Power, More…
Toll Free: 866-379-2600


Abrasives Inc.
Check our Prices for Blast Abrasives

Faced with higher abrasive costs? We invite you to call & check our rates on Black Magic® coal slag and other quality blast materials. Abrasives Inc. 800-584-7524


Wasser High-Tech Coatings Inc.
Wasser Coatings

have been used to protect some of the most important bridges in the country; learn about our NEPCOAT-approved system as well as our entire range of MCU coatings and Polyurea membranes.


DeHumidification Technologies
HUMIDITY PROBLEMS?

DH Tech has the most innovative and reliable equipment available to
control humidity efficiently
and effectively.
IT'S UNDER CONTROL!


US Minerals
US Minerals -
Black Magnum

With nationwide production and distribution capabilities, U.S. Minerals supplies a complete range of coal slag and other abrasives to meet all of your blasting needs.


Termarust Technologies
Termarust (HR CSA) Chemically Stops
Active Corrosion

Arch truss treated with Termarust's (HR CSA) in 2003. This steel arch bridge is rust free on all surfaces including the crevice corroded joints and connections.

 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker JPCL Europe

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2013, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com