D6132 Standard Test Method for Nondestructive Measurement of Dry Film Thickness of Applied Organic Coatings Over Concrete Using an Ultrasonic Gage

All Standards | ASTM Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date:
Updated On: July 29, 2008
Editorial Change:
 
1.1 This test method covers the use of ultrasonic film thickness gages to measure accurately and nondestructively the dry film thickness of organic coatings applied over a substrate of dissimilar material. Measurements may be made on field structures, on commercially manufactured products, or on laboratory test specimens. These types of gages can accurately measure the dry film thickness of organic coatings on concrete, wood and wallboard substrates.

1.2 This test method is not applicable to coatings that will be readily deformable under load of the measuring instrument as the instrument probe is placed directly on the coating surface to take a reading.

1.3 The effective range of instruments using the principle of ultrasonics is limited by gage design. A thickness range of 0.3 to 600 mils (8 µm to 15 mm) has been demonstrated.

1.4 The values stated in SI units are to be regarded as standard. No other units of measurement are included in this standard.

1.5 This standard does not purport to address the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.

(Back to all Standards)

 
   

Fox Industries Inc.
Repair, Protect & Strengthen

Need a coating? Turn to Fox. We have solutions to repair, protect and strengthen concrete, steel and wood substrates. Call 888-760-0369 or email info@foxind.com


Rapid Prep, LLC
Nation Wide Equipment Rentals

Rapid Prep, LLC is a full service provider of sandblasting & all other surface preparation equipment, with 60 years of experience within the industrial painting industry.


ANAFAPYT (Asociación Nacional de Fabricantes de Pinturas y Tintas)
ANAFAPYT Latin American
Coatings Show 2013

You are still on time to sign up
for Conferences, Exhibit Floor
and Short Course. Be part of
the best show in Latin
America. www.lacs2013.com


Corrosion Probe, Inc.
From Detection to Correction

Corrosion Probe, Inc. has the Most Concrete Coatings Experience and Expertise. Contact us today at
860-767-4402, www.cpiengineering.com


International Paint LLC
Our New Protective Coatings Centers

Our complete range of International and Devoe Coatings products are available at our Protective Coatings Centers, making purchases faster and easier.


JPCL - PCE - PaintSquare
Charter Advertising Opportunities Available through April 30.

Click above or contact Bernadette Landon
Publisher, JPCL Europe blandon@jpcleurope.com +1.412.697.0184
visit www.jpcleurope.com


Wasser High-Tech Coatings Inc.
Wasser Coatings

have been used to protect some of the most important bridges in the country; learn about our NEPCOAT-approved system as well as our entire range of MCU coatings and Polyurea membranes.

 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker JPCL Europe

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2013, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com