D4541 Standard Test Method for Pull-Off Strength of Coatings Using Portable Adhesion Testers

All Standards | ASTM Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date: August 16, 2010
Updated On: September 20, 2010
Editorial Change:
 
The pull-off strength of a coating is an important performance property that has been used in specifications. This test method serves as a means for uniformly preparing and testing coated surfaces, and evaluating and reporting the results. This test method is applicable to any portable apparatus meeting the basic requirements for determining the pull-off strength of a coating.

Variations in results obtained using different devices or different substrates with the same coating are possible (see Section 11). Therefore, it is recommended that the type of apparatus and the substrate be mutually agreed upon between the interested parties.

The purchaser or specifier shall designate a specific test method, that is, B, C, D, E, or F when calling out this standard.

(Back to all Standards)

 
   

Industrial Vacuum Equipment Corp.
Hurricane Vacuums
& Dust Collectors

Vacuum and dust collector hose, filters and related accessories.
IndustrialVacuum.com


SAFE Systems, Inc.
SAFE Systems'
Blast Lights &
Deadman Switches

Halogen or LED blast lights available with our NEW urethane bumper. Switches available in many colors for color coding your hoses.


Nationwide Overspray
Profession Overspray Removal Services

The Finest Name in Safe Overspray Removal. We specialize in removing all contaminants from any surface. Family Owned and Operated for 33 years! Fully insured. Satisfaction is guaranteed.


N.T. Ruddock Co.

Our Abrasives Hold Up Under Pressure

N. T. Ruddock focuses on abrasive selection, equipment evaluation, equipment maintenance & reduction of abrasive consumption. Other services include Screen Analysis & Background Radiation Testing.


SEMicro Division, M.E. Taylor Engineering, Inc.
Coatings Adhesion Testers

The PATTI® accurately measures the bond strength between coating & substrate. Outfitted properly, the surface can be rough, porous, or curved & >10K psi strong!


Wasser High-Tech Coatings Inc.
Wasser Coatings Protect

Wasser Coatings offer a complete range of Moisture Cure Urethane (NEPCOAT approved) systems in addition to Polyurea membranes and linings(NSF).
www.wassercoatings.com


WINOA Group
W Abrasives : Shot Peening Solutions

W Abrasives has developed an exclusive range of products to boost your peening and blasting performances.


DeHumidification Technologies
HUMIDITY PROBLEMS?

DH Tech has the most innovative and reliable equipment available to
control humidity efficiently
and effectively.
IT'S UNDER CONTROL!


Novetas Solutions
Number 1 Crushed Glass Abrasive in America!

Manufactured from 100% Recycled Glass.
NO Crystalline Silica,
Beryllium & Arsenic
Great White Metal Finish!
4 plants on Navy QPL
Call us at 866-775-6226


US Minerals
US Minerals -
Black Magnum

With nationwide production and distribution capabilities, U.S. Minerals supplies a complete range of coal slag and other abrasives to meet all of your blasting needs.

 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2016, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com