SSPC-SP 1, Solvent Cleaning

All Standards | SSPC Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date: November 01, 1982
Updated On: April 01, 2002
Editorial Change: November 1, 2004
 
This specification covers the requirements for the solvent cleaning of steel surfaces

(Back to all Standards)

 
   

Graco Inc.
The Fastest Way
to Touch-Up

The ProShot® HD cordless sprayer for spot repair, small jobs and touch-up. Easily sprays the toughest protective and marine coatings (up to 100% solids).


DeFelsko Corporation
NEW PosiTector
Inspection Kits

PosiTector 6000 Coating Thickness Gage easily converts to a surface profile gage, dew point meter or ultrasonic wall thickness gage with a simple probe change.


Empire Scaffold
Work with a scaffold company you can trust

Empire Scaffold is a full-service scaffold company providing specialized, on-site support for the life of the project, with products & experience to keep your projects up & running, safely.


HoldTight Solutions Inc.
NO FLASH RUST -
NO CONTAMINANTS

Our HoldTight®102 salt remover & flash rush inhibitor prevents flash rust by removing surface contaminants.
Contact us for your nearest distributor. (800) 319.8802 sales@holdtight.com


Bullard

The Next Generation
of Blasting

• Lighest
• Coolest
• Most Comfortable
• Most Dependable


Clemco Industries Corp.
Powerful Protection in a Small Package

Mounts inside blast helmet, alerts operator to dangerous breathing-air condition by audible, visual, and vibratory alarms. Easily calibrated, battery operated.


TruQC, LLC
Click here to start your free trial

TruQC is cloud-based job-site documentation built for the iPad. It's easy-to-use, objective and complies to common industry standards. Learn more: TruQCApp.com.

 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker JPCL Europe

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2013, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com