B200-07 Sodium Chloride

All Standards | AWWA Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date:
Updated On: July 25, 2012
Editorial Change:
 
This standard covers sodium chloride in the form of rock, vacuum-granulated, compressed vacuum-granulated, solar, or compressed solar salt for use in the recharging of cation-exchange materials in water supply service for softening municipal and industrial water supplies. Additionally, sodium chloride is used in the recharging of anion-exchange materials for nitrate removal or dealkalization of municipal and industrial supplies. The purpose of this standard is to provide purchasers, manufacturers, and suppliers with the minimum requirements for sodium chloride, including physical, chemical, packaging, shipping, and testing requirements. Topics covered include: physical requirements; chemical requirements; impurities; verification; inspection; sampling; test procedures - general; moisture; insoluble matter; calcium; magnesium; sulfate; grease, fat, and oil; pH value; total impurities; sodium chloride assay; rejection; and, delivery.

(Back to all Standards)

 
   

Sherwin-Williams
Ask Sherwin-Williams

Does your Paint company know where your Paint is?
If your paint company is Sherwin-Williams it does.
Leave Nothing to Chance


Absolute Equipment/Grand Rental Station
Portable Power from Absolute Equipment

•Compressors
•Lighting Systems
•Generators
•Light Compaction
Sales • Rental • Service
Call 1-866-931-6655
Over a century of
providing excellence.


EDCO - Equipment Development Co. Inc.
We are American Made

Visit all of EDCO’s Internet homes:
EDCOINC.com
ContrxSystems.com
EDCOFabrication.com
YouTube Channel–search
EDCOincorporated
EDCO Twitter: @EDCOUSA 800-638-3326


Corrosion Specialties, Inc.
The T93R Airless
Tip System

is the longest lasting, highest quality tip and guard available to coatings applicators around the world. Click the link to contact Corrosion Specialties.


GMA Garnet USA
GMA Garnet™
Natural Abrasives

- Superior cleaning performance
- Even Profile
- Low Dust
- Cost-Effective
- Environmentally friendly
- Recyclable up to 5 times
Tel : +1 832 243 9300


Harsco
BLACK BEAUTY® GLASS

A 100% post-consumer bottle glass abrasive from a company you can trust. Toll Free: 1-888-733-3646


Safway Services
One Source. Every Solution.

The Safway Group is your source for multiservices. Painting, coating, insulation and more – all from the most trusted name in the industry.

 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker JPCL Europe

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2013, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com