D6886 Standard Test Method for Determination of the Individual Volatile Organic Compounds (VOCs) in Air-Dry Coatings by Gas Chromatography

All Standards | ASTM Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date: June 25, 2012
Updated On: October 01, 2012
Editorial Change:
 
In using Practice D3960 to measure the VOC content of waterborne coatings, precision tends to be poor for low VOC content air-dry coatings when the VOC weight fraction is determined indirectly. The present method first identifies and then quantifies the weight fraction of individual VOCs directly in air-dry coatings. The total VOC weight fraction can be obtained by adding the individual weight fraction values (Note 4).

Note 4—The present method may be used to speciate solvent-borne air-dry coatings. However, since these normally contain high, and often complex, quantities of solvent, precision tends to be better using the methods contained in Practice D3960, where the VOC fraction is determined by a direct weight loss determination.

SPME/GC makes it possible to identify very low levels of volatile compounds in a coating and could serve to make it possible to identify the presence of hazardous air pollutants (HAPs).

(Back to all Standards)

 
   

Sherwin-Williams
Ask Sherwin-Williams

Does your Paint company know where your Paint is?
If your paint company is Sherwin-Williams it does.
Leave Nothing to Chance


DeHumidification Technologies
HUMIDITY PROBLEMS?

DH Tech has the most innovative and reliable equipment available to
control humidity efficiently
and effectively.
IT'S UNDER CONTROL!


DRYCO
DEHUMIDIFICATION FOR
ANY SIZE PROJECT!

Temporary climate control equipment. Dehumidifiers,
Heaters, A/C, Power, More…
Toll Free: 866-379-2600


Mascoat
Global Leader In Thermal Insulating Coatings

Our coatings are uniquely engineered and manufactured in-house to fulfill market-specific needs, enhance energy retention, prevent CUI and protect personnel.


Dampney Co., Inc.
Rubber In a can!

Rubberized Spray in a
Handy Aerosol Can

• Stays flexible
• Seals off moisture penetration
• Non sagging formulation
• Will not crack, chip or peel
• Apply to wet and dry surfaces
• Paintable


Atlantic Design, Inc.
We’ve Got a Surprise For You!

We’ve designed two new lines
of equipment with shorter lead
times, budget friendly prices,
more safety features & all
with the same ADI quality!
866.Call.ADI


Axxiom Manufacturing
The Undisputed
Industry Leader.

Proven Innovation. Job Performance. Industry Training. Workplace Safety. Only Schmidt® abrasive blast equipment by Axxiom Manufacturing delivers it all!

 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker JPCL Europe

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2013, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com