SSPC-PA 2 Procedure for Determining Conformance to Dry Coating Thickness Requirements

All Standards | SSPC Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date:
Updated On: August 29, 2012
Editorial Change:
 
This standard describes a procedure for determining shop or conformance to a specified coating dry film thickness (DFT) range on ferrous and non-ferrous metal substrates using nondestructive coating thickness gages (magnetic and electronic) described in ASTM D 7091. The standard also contains a procedure to determine if dry coatings conform to specified requirements for minimum and maximum dry film thickness.

(Back to all Standards)

 
   

Oxford Instruments Coating Measurement
Oxford Instruments Coating Thickness Analyzers

Measure paint thickness/protective coatings using Oxford Instruments’ handheld and benchtop gauges, and XRF analyzers. Email industrial@oxinst.com or +1 800-447-4717


Bayer MaterialScience LLC
Desmodur® XP 2763 Drives Financial Results

High performance polyaspartic coatings
• Dry faster
• Fewer coats
• Superior corrosion/weather resistance
412-777-3983


TruQC, LLC
Click here to start your free trial

TruQC is cloud-based job-site documentation built for the iPad. It's easy-to-use, objective and complies to common industry standards. Learn more: TruQCApp.com.


Fischer Technology Inc.
Gauges Meet IMO-PSPC & SSPC-PA2 Requirements

• USB or optional Bluetooth
• Custom inspection reports
• Excellent on edges & rough surfaces; Optimum accuracy
• Largest selection of probes to meet challenging situations
Call Fischer: 800-243-8417


Abrasives Inc.
See the difference immediately Black Magic®

Quality blast abrasive goes farther. Use Black Magic® The Tough Stuff coal slag. Cleaner, consistent, less dust. Order yours today!
Abrasives Inc. 800-584-7524


ElektroPhysik
High-precision coating thickness gauge MiniTest 7400

MiniTest 7400 with intuitive menu control, enhanced data management with configuration assistent. Wear-resistant sensors for measuring tasks up to 35mm thickness.


Wasser High-Tech Coatings Inc.
Wasser Coatings

have been used to protect some of the most important bridges in the country; learn about our NEPCOAT-approved system as well as our entire range of MCU coatings and Polyurea membranes.

 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker JPCL Europe

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2013, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com