G10 Standard Test Method for Specific Bendability of Pipeline Coatings

All Standards | ASTM Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date: January 03, 2011
Updated On: February 02, 2011
Editorial Change:
 
This test will provide information on the ability of coatings applied to pipe to resist cracking, disbonding, or other mechanical damage as a result of bending. Because the test is applied to coated pipe from commercial production, the results can be directly used in the selection of similar materials for service. The test also has application as a quality control method when variations in coating application or material formulation will affect bending performance.

1.1 This method covers the specific determination of the effect of short-radius bends on coatings applied to 33.4-mm (1-in. nominal) diameter pipe.

(Back to all Standards)

 
   

STOPAQ
Click here if you
Dare to Compare

Permanent Visco-Elastic Corrosion Prevention Traditional systems versus Stopaq Solutions.


LS Industries
LS Blasters: Optimum Steel Cleaning Efficiency

Simplify surface prep with the precise shot control of LS Blasters. Our blast technology delivers optimum coverage and finish. 800-533-8008


Denso North America Inc.
Denso SeaShield
Marine Systems

A full range of steel, concrete and timber pile rehabilitation systems including petrolatum systems, fiberglass jackets, epoxy grouts and many other product lines.
Call 1-281-821-3355 or Visit densona.com


Cardolite Corporation
CNSL Based Products

Renewable CNSL epoxy curing agents and resins with fast cure at low temperature, adhesion to unprepared surfaces and excellent corrosion and water protection.


MSA (The Safety Company)
Free Whitepaper: A Quick Guide to Air-Purifying Respirators

Download a whitepaper on air-purifying respirators and powered air-purifying respirators from the safety experts at MSA.


ITW Polyspec
FLEX IMO
for Marine Deck Coating

FLEX IMO is a uniquely formulated decorative polymer deck coating system that combines aesthetics and fire safety. FLEX IMO is an IMO approved coating system.


Microban International Ltd.
Cleaner Paint with Microban Antimicrobial Protection

Microban, the leader in built-in antimicrobial protection, inhibits the growth of stain and odor causing bacteria, mold and mildew in paint products.

 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker JPCL Europe

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2013, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com