D4139 Standard Guide for Determining Volatile and Nonvolatile Content of Pigments

All Standards | ASTM Standards
Search Standards

Click to Purchase and Download this Standard or Test Method

Revision Date: June 22, 2009
Updated On: September 30, 2009
Editorial Change:
The nonvolatile content of raw materials may be used to determine the total nonvolatile content (solids) of paint and related coatings. Such information may be useful to coatings producers and users for the determination of the total solids available for film formation and for the estimation of the volatile organic content.

(Back to all Standards)

Industrial Vacuum Equipment Corp.
Hurricane Vacuums
& Dust Collectors
Vacuum and dust collector hose, filters and related accessories.

SAFE Systems, Inc.
Custom blast rooms
by SAFE Systems
Don't waste time and money "making do" with a "standard" design. Let us work with you to design and build the system that best fits your requirements.
Call 1-800-634-7278

SABRE Autonomous Solutions
The ALPHA1 provides reliable results consistently allowing you to cost your next job with confidence.

Tarps manufacturing, Inc.
QUALITY MADE IN AMERICA —Available near you!
CLICK to get a behind-the-scenes look at how Tarps Manufacturing makes the highest-quality tarps right here in the USA — available nationwide.

Vector Technologies Ltd.
The Original Performance Proven Vacuum Solutions
VecLoader® 616 Double Dump, Continuous Vacuum, 170 HP w/ 2,400 CFM & 28” Hg. 33% More Efficient than traditional vacuum systems! Choose Vector for the most powerful and the most reliable trailer mounted vacuums in the industry! Email us at: or call us at: 800-832-4010

Sky Climber, LLC
Solutions in Suspended Access
Safely reach workspaces regardless of size or purpose with our full line of Hoists, modular Platforms, and versatile Workcages.

NLB Corporation
NLB Sure Shroud: Greater Protection and Flexibility
NLB’s Sure Shroud’s lighter weight and flexibility reduces operator fatigue and offers unmatched protection against high pressure hose ruptures. 10k to 40k psi rated.

Jotun Paints Inc.
Jotun Jotachar 1709
Mesh-free passive fire protection epoxy designed to protect against hydrocarbon pool fire scenarios for up to four hours as defined in the ANSI/UL1709 standard.

Novatek Corporation
Dustless Coatings Removal
Novatek Corporation, Dustless Coatings Removal Strip, clean and profile all dust free! Comply with new lead standards. Contact today: (866) 563-7800

Graco Inc.
Graco EcoQuip 2: Experience the Difference
While others claim their equipment is the same, none of them compare to Graco’s EcoQuip 2™ Vapor Abrasive® blasting line. Visit to learn more.


Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL

The Technology Publishing Network

Durability + Design PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us