D1730 Standard Practices for Preparation of Aluminum and Aluminum-Alloy Surfaces for Painting

All Standards | ASTM Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date: May 18, 2009
Updated On: May 27, 2009
Editorial Change:
 
1.1 These practices cover four types of treatment for preparation of aluminum and aluminum-alloy surfaces for painting, as follows: 1.1.1 Type A—Solvent Cleaning. 1.1.2 Type B—Chemical Treatments. 1.1.3 Type C—Anodic Treatments. 1.1.4 Type D—Mechanical Treatments. These four types cover a number of procedures, as described herein.

1.2 Variations in surface treatment produce end conditions which differ, and which do not necessarily yield identical results when paints are applied. Service conditions will dictate the type of surface preparation that should be selected, although the quality produced by any individual method may vary with different alloys.

(Back to all Standards)

 
   

GMA Garnet USA
GMA Garnet™
Natural Abrasives

- Superior cleaning performance
- Even Profile
- Low Dust
- Cost-Effective
- Environmentally friendly
- Recyclable up to 5 times
Tel : +1 832 243 9300


Clemco Industries Corp.
Powerful Protection in a Small Package

Mounts inside blast helmet, alerts operator to dangerous breathing-air condition by audible, visual, and vibratory alarms. Easily calibrated, battery operated.


LS Industries
LS Blasters: Optimum Steel Cleaning Efficiency

Simplify surface prep with the precise shot control of LS Blasters. Our blast technology delivers optimum coverage and finish. 800-533-8008


Van Air Systems
The Blast Pak

Van Air Systems' portable desiccant air dryer. Get dry compressed air with this All-In-One blasting and coating solution.


MMLJ
Superfast Dustless Abrasive Blasting - Watch Video

Dustless Blasting creates no dust plume so others can work nearby unaffected. Maximize Productivity! Watch our numerous YouTube videos to learn more.


Absolute Equipment/Grand Rental Station
Portable Power from Absolute Equipment

•Compressors
•Lighting Systems
•Generators
•Light Compaction
Sales • Rental • Service
Call 1-866-931-6655
Over a century of
providing excellence.


Industrial Vacuum Equipment Corp.
Hurricane Vacuums
& Dust Collectors

Vacuum and dust collector hose, filters and related accessories.
IndustrialVacuum.com

 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker JPCL Europe

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2013, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com