C283 Standard Test Methods for Resistance of Porcelain Enameled Utensils to Boiling

All Standards | ASTM Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date:
Updated On: October 07, 2008
Editorial Change:
 
1.1 These test methods cover the determination of the resistance of porcelain enamel coatings used on utensils to attack by boiling acid.

1.2 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.

(Back to all Standards)

 
   

Oxford Instruments Coating Measurement
Oxford Instruments Coating Thickness Analyzers

Measure paint thickness/protective coatings using Oxford Instruments’ handheld and benchtop gauges, and XRF analyzers. Email industrial@oxinst.com or +1 800-447-4717


MMLJ
Superfast Dustless Abrasive Blasting - Watch Video

Dustless Blasting creates no dust plume so others can work nearby unaffected. Maximize Productivity! Watch our numerous YouTube videos to learn more.


TruQC, LLC
Click here to start your free trial

TruQC is cloud-based job-site documentation built for the iPad. It's easy-to-use, objective and complies to common industry standards. Learn more: TruQCApp.com.


Blastox/The TDJ Group, Inc.
Blastox - One Step
Lead Abatement

Don't waste $$ on added labor steps with other methods. Don't mix, meter or apply at the job-site. Avoid strict hazardous waste rules.
Let your painters paint!


Fischer Technology Inc.
Gauges Meet IMO-PSPC & SSPC-PA2 Requirements

• USB or optional Bluetooth
• Custom inspection reports
• Excellent on edges & rough surfaces; Optimum accuracy
• Largest selection of probes to meet challenging situations
Call Fischer: 800-243-8417


Hempel (USA) Inc.
Real Coating
for Real Protection

Hempel's protective coatings cover a wide range of applications across multiple industries from oil and gas to power generation to infrastructure.


Safety Lamp of Houston, Inc.
Wet & hazardous area lighting solutions from SAFETY LAMP of Houston

New WOLF LED and fluorescent lights are now available, including low voltage tank lighting kits.
Call: (281) 964-1019.

 
 
 
Technology Publishing

The Technology Publishing Network

The Journal of Protective Coatings & Linings (JPCL) PaintSquare
Durability + Design Paint BidTracker JPCL Europe

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy policy   |   Terms & conditions   |   Site Map   |   Search   |   Contact Us
 

© Copyright 2000-2013, Technology Publishing / PaintSquare, All rights reserved
2100 Wharton Street, Suite 310, Pittsburgh PA 15203-1951; Tel 1-412-431-8300; Fax 1-412-431-5428; E-mail webmaster@paintsquare.com